Processing Properties Metric English Comments
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Kraton® G7705 GI-B (SEBS) Compound
Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Kraton® G7705 GI-N (SEBS) Compound
Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Kraton® G7820 GU-N (SEBS) Compound
Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 4107 C Black TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 4400 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 4701 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 2599 TPE Thermoplastic Elastomer
This material bonds to polypropylene. Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame Retardant Flexibility, GoodHeat StabilizedOzone ResistantPr..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 8030 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® D 3804 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber
AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets.
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Kraton® G7720 GI-N (SEBS) Compound
Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..