Polymer Property : Injection Pressure = 83.36 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 39.23 - 83.36 MPa
5690 - 12090 psi
Second
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..