Polymer Property : Injection Pressure = 90.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Plastcom PLASTALEN® PH 69 GF 30 Polypropylene reinforced with glass fiber
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl..
Injection Pressure 50.0 - 90.0 MPa
7250 - 13100 psi
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized
PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo..
Injection Pressure 70.0 - 90.0 MPa
10200 - 13100 psi
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded
PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application..
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner JEPP2007 PP For Automotive Parts
Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner JEPP2056 PP For Automotive Parts
Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 40.0 - 90.0 MPa
5800 - 13100 psi
Zhejiang Juner JEPPBC001 Weatherability PP Series
Applications: Weatherability ProductsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 40.0 - 90.0 MPa
5800 - 13100 psi
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 40.0 - 90.0 MPa
5800 - 13100 psi
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP201-G30 PP For Automotive Parts
Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP430R Weatherability PP Series
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP6-1JE PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP8 PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 50.0 - 90.0 MPa
7250 - 13100 psi
Toyobo GLAMIDE® TY-791HT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Beijing Chemical Industry KAIFA® HN201-G0 PA6 Resin
Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl..
Injection Pressure 60.0 - 90.0 MPa
8700 - 13100 psi
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin
Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)