Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled
30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc.
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified
V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc.
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
Vent Depth 0.00127 - 0.00203 cm
0.000500 - 0.000800 in
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc.
Vent Depth 0.00127 - 0.00203 cm
0.000500 - 0.000800 in
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend
Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc.
Vent Depth 0.00127 - 0.00254 cm
0.000500 - 0.00100 in
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.