Polymer Property : Vent Depth = 0.00381 cm Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-1000 High Flow PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT
General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Vent Depth 0.00254 - 0.00381 cm
0.00100 - 0.00150 in
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy
A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color ..