Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.1016 - 0.127 cm | 0.04000 - 0.0500 in | |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |