Die Opening 0.200 cm
0.0787 in
Chevron Phillips mPact™ D449 HDPE Blown Film Resin  (discontinued **)
Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw..