Processing Properties Metric English Comments
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Blow Film Extrusion
Braskem CN8092 EVA Molding Copolymer
CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i..
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..