Hot-Working Temperature | 538 °C | 1000 °F | Flow Stress of 65 MP at 3.6s<sup>-1<sup> |
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
Hot-Working Temperature | 538 °C | 1000 °F | Flow Stress of 95 MP at 3.6s<sup>-1<sup> |
Schmolz + Bickenbach IMRE™ Stainless Steel Bar Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand.. |