Polymer Property : Hot-Working Temperature = 954 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hot-Working Temperature 954 - 1180 °C
1750 - 2150 °F
Forging range
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Hot-Working Temperature 954 - 1180 °C
1750 - 2150 °F
Forging range
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..
Hot-Working Temperature 954 - 1200 °C
1750 - 2200 °F
Forging range
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
Hot-Working Temperature 954 - 1200 °C
1750 - 2200 °F
Forging range
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
Hot-Working Temperature 954 - 1200 °C
1750 - 2200 °F
Forging range
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
Hot-Working Temperature >= 954 °C
>= 1750 °F
Forge
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar
Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu..