Polymer Property : Head Temperature = 140 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 140 - 160 °C
284 - 320 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Head Temperature >= 140 °C
>= 284 °F
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation
Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of..
Head Temperature 140 - 185 °C
284 - 365 °F
Average value: 174 °C Grade Count:10
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..