Polymer Property : Head Temperature = 194 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 70.0 - 90.0 °C
158 - 194 °F
3M Dyneon™ PFE 300Z Clear Perfluoroelastomer System
Features and Benefits:Proprietary polymer and catalyst system enables the manufacture of optically clear finished partsProportionate polymer and catalyst package simplifies the mixing processLow ext..
Head Temperature 70.0 - 90.0 °C
158 - 194 °F
3M Dyneon™ 301Z Translucent Perfluoroelastomer System
Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica..