Polymer Property : Head Temperature = 347 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 175 - 215 °C
347 - 419 °F
Blow Molding
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound
HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900..