Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 1.00 - 1.33 min | 1.00 - 1.33 min | |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |