Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 11.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 11.0 - 12.0 min
11.0 - 12.0 min
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the ..
Copyright © lookpolymers.com All Rights Reserved