Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 18.0 min @Temperature 25.0 °C |
18.0 min @Temperature 77.0 °F |
|
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. Thi.. |