Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 99999 min @Temperature 25.0 °C |
99999 min @Temperature 77.0 °F |
Indefinite working life at 25°C (100 g) |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |
|||
Pot Life | 99999 min @Temperature 25.0 °C |
99999 min @Temperature 77.0 °F |
Indefinite working life at 25°C (100 g) |
Armstrong A-702 Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Pot Life | 99999 min @Temperature 25.0 °C |
99999 min @Temperature 77.0 °F |
Indefinite working life at 25°C (100 g) |
Armstrong A-706 Epoxy Adhesive A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m.. |