Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 200 °C @Time 10800 - 14400 sec |
392 °F @Time 3.00 - 4.00 hour |
or |
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist.. |
|||
Drying Temperature | 200 °C @Time 10800 - 14400 sec |
392 °F @Time 3.00 - 4.00 hour |
or |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |