Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 90.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 32.2 - 37.8 °C

@Time 7200 - 10800 sec
90.0 - 100 °F

@Time 2.00 - 3.00 hour
out of sealed box
Green Dot Terratek® Flex GDH-B1 Compostable Bioplastic Elastomer
GDH-B1 is an elastomeric bioplastic with a diverse range of potential applications. It is a starch-based elastomer that is strong, durable and pliable with an exquisite soft touch. The bioplastic i..