Processing Properties Metric English Comments
Zone 4-x 121 - 132 °C
250 - 270 °F
LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound
ApplicationsPETROTHENE YR 19513 is a colorable, thermoplastic, non-halogenated, flame retardant polyolefin compound designed for use as striping for chemically crosslinkable automotive primary and a..