Polymer Property : Zone 4-x = 216 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4-x 216 - 221 °C
420 - 430 °F
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm..