Processing Properties Metric English Comments
Adapter Temperature 165 - 175 °C
329 - 347 °F
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Adapter Temperature 165 - 175 °C
329 - 347 °F
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging
The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan..
Adapter Temperature 165 - 185 °C
329 - 365 °F
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th..
Adapter Temperature 165 °C
329 °F
5, Extrusion
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av..