Processing Properties Metric English Comments
Adapter Temperature 215 - 235 °C
419 - 455 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 215 °C
419 °F
Taiwan PU Corporation TPU-E98 General Grade, Extrusion Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 215 °C
419 °F
Taiwan PU Corporation TPUI-ED64 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 215 °C
419 °F
Taiwan PU Corporation TPUI-T64D Transparent Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.