Processing Properties Metric English Comments
Die Temperature 120 °C
248 °F
Borealis LE0520 Polyethylene Compound, Crosslinkable, Semiconductive
LE0520 is a Strippable Semi conductive Insulation Shielding for Power Cables. LE0520 is suitable for use in triple extrusion processes. Strip forces in the range of 3-6 kN/m (7-14 lbs/half inch) ha..
Die Temperature >= 120 °C
>= 248 °F
Borealis Low Sulfur™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Low Sulphur LE0594 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me..
Die Temperature >= 120 °C
>= 248 °F
Borealis Low Sulfur™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Low Sulphur LE0595 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me..