Die Temperature 218 °C
424 °F
Zone 1, Extrusion
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
Die Temperature 218 °C
424 °F
Zone 2, Extrusion
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
Die Temperature 218 °C
424 °F
6, Zone 1, Extrusion
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
Die Temperature 218 °C
424 °F
Zone 2, Extrusion
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..