Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 232 - 246 °C | 450 - 475 °F | |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |