Processing Properties Metric English Comments
Die Temperature 208 °C
406 °F
Extrusion
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 208 °C
406 °F
Extrusion
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..