Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 230 °C | 446 °F | |
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Die Temperature | 230 °C | 446 °F | Zone 5 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Die Temperature | 230 °C | 446 °F | Zone 2 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Die Temperature | 230 °C | 446 °F | Zone 2 |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | (6) Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Temperature | 230 °C | 446 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE. |