Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 110 °C | 230 °F | |
Braskem BF 0323/12 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323/12 is a high molecular weight LDPE produced under high pressure technology. Films obtained with this product show outstanding optical properties, excellent mechanical properties,.. |
|||
Zone 1 | 110 °C | 230 °F | |
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating proces.. |