Polymer Property : Zone 1 = 323 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 162 - 191 °C
323 - 375 °F
Entec Hyril® GP355AS Styrene Acrylonitrile
Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec