Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0778/BK Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0916 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7868 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7908 Polyphthalamide, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-7970 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8302 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Zone 1 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec.. |
|||
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Zone 1 | 300 - 340 °C | 572 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |