Processing Properties Metric English Comments
Zone 1 176 °C
349 °F
Extrusion
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo..
Zone 1 176 °C
349 °F
Extrusion
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane
Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by ..