Polymer Property : Zone 2 = 120 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 100 - 120 °C
212 - 248 °F
Compression
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane
Pearlbondâ„¢ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli..