Polymer Property : Zone 2 = 221 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 105 °C
221 °F
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid..