Processing Properties Metric English Comments
Zone 2 280 °C
536 °F
Compression
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
Zone 2 280 °C
536 °F
Compression
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
Zone 2 280 °C
536 °F
Compression
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin..