Polymer Property : Screw Cooling Temperature = 194 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEM”; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki..
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Average value: 80.0 °C Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..