Processing Properties Metric English Comments
Zone 3 107 - 113 °C
225 - 235 °F
Zone 3-X
LyondellBasell Petrothene® XL07425 Copolymer
ApplicationsPETROTHENE XL07425 is especially formulated for use in flame retardant primary insulation for low voltage automotive wire and cable applications (SAE J1128). Non-discoloring antioxidant ..