Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 204 - 232 °C | 400 - 450 °F | |
LyondellBasell Alathon® M5370WC High Density Polyethylene ApplicationsALATHON M 5370WC is a natural, high density, polyethylene copolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cab.. |
|||
Zone 3 | 204 - 232 °C | 400 - 450 °F | |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Zone 3 | 204 - 232 °C | 400 - 450 °F | |
LyondellBasell Petrothene® LR590001 High Density Polyethylene ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e.. |
|||
Zone 3 | 204 - 232 °C | 400 - 450 °F | |
LyondellBasell Petrothene® LR590005 High Density Polyethylene ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains .. |
|||
Zone 3 | 204 - 232 °C | 400 - 450 °F | |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |