Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 315 °C | 599 °F | Metering-zone |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Zone 3 | 315 °C | 599 °F | Metering-zone |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |