Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 200 °C | 392 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
Zone 3 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 3 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 3 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Zone 3 | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical SH610S ABS, Excellent Surface, High Impact Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Zone 3 | 200 - 220 °C | 392 - 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Zone 3 | 200 °C | 392 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil.. |
|||
Zone 3 | 200 °C | 392 °F | Extrusion |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | Injection |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 3 | 200 - 210 °C | 392 - 410 °F | Injection |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Zone 3 | 200 - 240 °C | 392 - 464 °F | |
Eurostar Starglas CF006 Styrenic, 30% Glass Filled, Injection Molding Starglas CF006 is a 30% Glass Fiber Reinforced Styrenic Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 200 °C | 392 °F | Extrusion |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 3 | 200 °C | 392 °F | Extrusion |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 3 | 200 °C | 392 °F | Extrusion |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 3 | 200 °C | 392 °F | Metering-zone |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Zone 3 | 200 - 225 °C | 392 - 437 °F | |
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC.. |
|||
Zone 3 | 200 °C | 392 °F | Metering-zone |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Zone 3 | 200 °C | 392 °F | Extrusion |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |
|||
Zone 3 | 200 °C | 392 °F | Metering-zone |
BASF Ultraform® N2520 XL2 POM Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF |
|||
Zone 3 | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 3 | 200 °C | 392 °F | Metering-zone |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |