Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 115 °C | 239 °F | |
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid.. |