Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A3Z BK 30464 PA66 (Conditioned) Description: Impact-modified and stabilized injection- molding grade for components and housings with good low temperature impact resistance.Information provided by BASF |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Zone 4 | 290 °C | 554 °F | Nozzle |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |