Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 982 - 1070 °C | 1800 - 1950 °F | Pouring Range |
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy Information provided by IBC Advanced Alloys. |
|||
Casting Temperature | 982 - 1070 °C | 1800 - 1950 °F | Pouring Range |
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy 21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys. |
|||
Casting Temperature | 970 - 1070 °C | 1780 - 1960 °F | |
Wieland 1416 Wilaform Gold Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDen.. |
|||
Casting Temperature | 970 - 1070 °C | 1780 - 1960 °F | |
Wieland 1001 Wilaform Gold Hard 333/standard yellow gold alloy. Particularly suited for strongly stressed parts.Applications: casting, laminar decoration, pipes, tubingDental |