Polymer Property : Casting Temperature = 1940 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 1060 - 1160 °C
1940 - 2120 °F
Wieland 1103 Wilaform Gold
Hard yellow gold alloy particularly suitable for decoration casting.Applications: casting, laminar decorationDental
Casting Temperature 1060 °C
1940 °F
Wieland Auropal 1 Casting Alloy
Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental