Polymer Property : Casting Temperature = 2010 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 1000 - 1100 °C
1830 - 2010 °F
Wieland 1605 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental
Casting Temperature 1000 - 1100 °C
1830 - 2010 °F
Wieland 3012 Wilaform Silver
A balance of manufacturing and performance characteristics makes this the preferential silver alloy in the decoration manufacturing industry. The alloy unites good ductility properties with the nec..
Casting Temperature 1010 - 1100 °C
1850 - 2010 °F
Wieland 3013 Wilaform Silver
Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental