Processing Properties Metric English Comments
Casting Temperature 1010 - 1110 °C
1850 - 2030 °F
Wieland 1007 Wilaform Gold
Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Casting Temperature 1010 - 1110 °C
1850 - 2030 °F
Wieland 1023 Wilaform Gold
Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental
Casting Temperature 1010 - 1110 °C
1850 - 2030 °F
Wieland 1602 Wilaform Gold
Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu..