Polymer Property : Casting Temperature = 2050 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 1020 - 1120 °C
1870 - 2050 °F
Wieland 1403 Wilaform Gold
Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin..