Processing Properties Metric English Comments
Casting Temperature 1950 - 2150 °C
3540 - 3900 °F
Wieland 1746 Wilaform Platinum
Platinum alloy particularly suitable for decoration castingApplications: casting, laminar decoration, tubingDental
Casting Temperature 1950 - 2150 °C
3540 - 3900 °F
Wieland 1757 Wilaform Platinum
Platinum alloy without nickel, low-priced for all kinds of decoration productionApplications: chains, laminar decoration, pipes, tubingDental