Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 9.00 °C | 48.2 °F | |
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin.. |