Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.100 - 0.150 min @Temperature 204 °C |
0.100 - 0.150 min @Temperature 399 °F |
|
3M Scotchkote™ 412 Fusion Bonded Epoxy Coating 3M Scotchkote Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to preheated steel.. |